Drive transmissions axle shaft induction hardening

Induction surface hardening followed by self-tempering by cooling

· induction hardening

IGBT Induction Heat Treatment Process Parameters:
Effective hardening depth: 3.5÷5 mm
Total hardening depth: 4.5÷6 mm
Surface hardness after hardening: 505÷2 HRC
Cycle time: 18 sec

axle shaft induction hardening